China Cheap Price Inconel Alloy Tubes - Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Seamless Pipe, Sheet, Wire – Guojin
China Cheap Price Inconel Alloy Tubes - Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Seamless Pipe, Sheet, Wire – Guojin Detail:
Available Products
Seamless tube, Plate, Rod, Forgings, Fasteners, Pipe Fittings
Production Standards
Product |
ASTM |
Bars and Forgings |
B 637 |
Chemical Composition
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
S |
Ti |
Nb+Ta |
Al |
Co |
Cu |
Min |
70.0
|
14.0 |
5.0 |
|
|
|
|
2.25 |
0.70 |
0.40 |
|
|
Max |
17.0 |
9.0 |
0.08 |
1.00 |
0.50 |
0.010 |
2.75 |
1.20 |
1.00 |
1.00 |
0.50 |
Physical Properties
Density |
8.28 g/cm3 |
Melting |
1393-1427℃ |
Inconel X-750 Features
Inconel X-750 alloy is mainly a nickel-based superalloy which is age-strengthened with γ[Ni3(Al, Ti, Nb)] phase. It has good corrosion resistance and oxidation resistance below 980℃, and below 800℃ It has high corrosion resistance. It has good relaxation resistance below 540°C, as well as good formability and weldability. This alloy is mainly used for the manufacture of aircraft engines that work below 800°C and require high strength. . Springs can also be used to manufacture steam turbine turbine blades and other parts, such as plates, strips, bars, forgings, rings, wires, pipes, etc.
Inconel X-750 Heat Treatment Process
The solution heat treatment system for plates, strips and pipes in the supply state is 980℃±15℃, air cooling. For the intermediate heat treatment system of materials and parts, the following processes can be selected for heat treatment.
Annealing: 955~1010℃, water cooling.
Annealing of welded parts before welding: 980℃, 1h.
Stress relief annealing of welded parts: 900℃, moisturizing for 2h.
Stress relief annealing: 885℃±15℃, 24h, air cooling.
Inconel X-750 Available Varieties and Specifications
Bars, forgings, rings, hot-rolled sheets, cold-rolled sheets, strips, tubes and wires can be supplied in various sizes.
Plates and strips are generally supplied after hot or cold rolling, annealing or solution, pickling and polishing.
Bars, forgings and rings can be supplied in the forged or hot rolled state; they can also be supplied in solution treatment after forging; bars can be supplied after solution and polished or turned, and can be supplied in cold when the order requires Pull state into place.
The wire can be supplied in the solid solution state; for the wire with a nominal diameter or thickness below 6.35mm, it can be solid solution and supplied with a cold drawing deformation of 50% to 65%; the nominal diameter or side length is greater than 6.35mm. Wire, after solution treatment, is supplied with a cold-drawing deformation of not less than 30%. For wires with a nominal diameter or side length not greater than 0.65mm, they can be supplied with a cold-drawing deformation of not less than 15% after solution treatment as required.
Inconel X-750 Application Areas
The alloy is mainly used for the manufacture of leaf springs and coil springs with high strength requirements and relaxation resistance for aero-engines operating below 800°C. It can also be used to make parts such as turbine blades. Available varieties are sheet, strip, bar, forging, ring, wire and tube.
Product detail pictures:



Related Product Guide:
To be able to give you benefit and enlarge our business, we also have inspectors in QC Team and assure you our greatest service and products for China Cheap Price Inconel Alloy Tubes - Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Seamless Pipe, Sheet, Wire – Guojin , The product will supply to all over the world, such as: Iran, New Zealand, Senegal, We guarantee that our company will try our best to reduce customer purchase cost , shorten the period of purchase , stable products quality , increase customers' satisfaction and achieve win-win situation .

The customer service staff is very patient and has a positive and progressive attitude to our interest, so that we can have a comprehensive understanding of the product and finally we reached an agreement, thanks!