China Gold Supplier For Inconel 617 Tubes - Superalloy Inconel625/ UNS N06625/ Alloy625 Manufacturer – Guojin
China Gold Supplier For Inconel 617 Tubes - Superalloy Inconel625/ UNS N06625/ Alloy625 Manufacturer – Guojin Detail:
Available Products
Seamless tube, Plate, Rod, Forgings, Fasteners, Pipe Fittings
Production Standards
Product |
ASTM |
Bar |
B 446 |
Plate, Sheet and Strip |
B 443, B 906 |
Seamless pipe,tube |
B 444, B 829 |
Welded pipe |
B 705, B 775 |
Welded fittings |
B 704, B 751 |
Welded connectors |
B 366 |
Forged billets and bars |
B 472 |
Forging |
B 564 |
Chemical Composition
% |
Ni |
Cr |
Mo |
Fe |
C |
Mn |
Si |
P |
S |
Co |
Nb+Ta |
Al |
Ti |
Min |
58.0 |
20.0 |
8.0 |
|
|
|
|
|
|
|
3.15 |
|
|
Max |
|
23.0 |
10.0 |
5.0 |
0.10 |
0.50 |
0.50 |
0.015 |
0.015 |
1.00 |
4.15 |
0.40 |
0.40 |
Physical Properties
Density |
8.36 g/cm3 |
Melting |
1330-1375℃ |
Inconel 625 Features
1. Excellent corrosion resistance to various corrosive media in oxidizing and reducing environments
2. Excellent resistance to pitting corrosion and crevice corrosion, and will not produce chloride ion stress corrosion cracking
3. Excellent corrosion resistance to inorganic acids, such as nitric acid, phosphoric acid, sulfuric acid, hydrochloric acid and mixed acids of sulfuric acid and hydrochloric acid, etc.
4. Excellent resistance to corrosion of various inorganic acid mixed solutions
5. When the temperature reaches 40℃, it can show good corrosion resistance in various concentrations of hydrochloric acid solution
6. Good workability and weldability, no post-weld cracking sensitivity
7. Manufacture certification of pressure vessels with wall temperature of -196~450℃
8. Certified by the American Society of Corrosion Engineers NACE standard (MR-01-75) to meet the highest standard level VII for use in sour gas environments.
Inconel625 Application Areas
The softened and annealed low carbon alloy 625 is widely used in the chemical process industry, and its better corrosion resistance and high strength enable it to be used as a thinner structural component. Alloy 625 can be used in applications exposed to seawater and subject to high mechanical stress. Typical application areas:
1. Components of organic chemical processes containing chlorides, especially where acid chloride catalysts are used
2. Digesters and bleaching tanks for the pulp and paper industry
3. Absorption tower, reheater, flue gas inlet baffle, fan (humid), agitator, deflector and flue in flue gas desulfurization system
4. For the manufacture of equipment and components for use in sour gas environments
5. Acetic acid and acetic anhydride reaction generator
6. Sulfuric acid condenser
Product detail pictures:


Related Product Guide:
Our company puts emphasis on the management, the introduction of talented personnel, and the construction of staff building, trying hard to improve the quality and liability consciousness of staff members. Our company successfully attained IS9001 Certification and European CE Certification of China Gold Supplier For Inconel 617 Tubes - Superalloy Inconel625/ UNS N06625/ Alloy625 Manufacturer – Guojin , The product will supply to all over the world, such as: Rome, Johannesburg, Jordan, If you are for any reason unsure which product to select, do not hesitate to contact us and we will be delighted to advise and assist you. This way we will be providing you with all the knowledge needed to make the best choice. Our company strictly follows Survive by good quality, Develop by keeping good credit. operation policy. Welcome all the clients old and new to visit our company and talk about the business. We are looking for more and more customers to create the glorious future.

The company has rich resources, advanced machinery, experienced workers and excellent services, hope you keep improving and perfecting your products and service, wish you better!