Discount Price Inconel 690 Tubes - Superalloy Inconel625/ UNS N06625/ Alloy625 Manufacturer – Guojin
Discount Price Inconel 690 Tubes - Superalloy Inconel625/ UNS N06625/ Alloy625 Manufacturer – Guojin Detail:
Available Products
Seamless tube, Plate, Rod, Forgings, Fasteners, Pipe Fittings
Production Standards
Product |
ASTM |
Bar |
B 446 |
Plate, Sheet and Strip |
B 443, B 906 |
Seamless pipe,tube |
B 444, B 829 |
Welded pipe |
B 705, B 775 |
Welded fittings |
B 704, B 751 |
Welded connectors |
B 366 |
Forged billets and bars |
B 472 |
Forging |
B 564 |
Chemical Composition
% |
Ni |
Cr |
Mo |
Fe |
C |
Mn |
Si |
P |
S |
Co |
Nb+Ta |
Al |
Ti |
Min |
58.0 |
20.0 |
8.0 |
|
|
|
|
|
|
|
3.15 |
|
|
Max |
|
23.0 |
10.0 |
5.0 |
0.10 |
0.50 |
0.50 |
0.015 |
0.015 |
1.00 |
4.15 |
0.40 |
0.40 |
Physical Properties
Density |
8.36 g/cm3 |
Melting |
1330-1375℃ |
Inconel 625 Features
1. Excellent corrosion resistance to various corrosive media in oxidizing and reducing environments
2. Excellent resistance to pitting corrosion and crevice corrosion, and will not produce chloride ion stress corrosion cracking
3. Excellent corrosion resistance to inorganic acids, such as nitric acid, phosphoric acid, sulfuric acid, hydrochloric acid and mixed acids of sulfuric acid and hydrochloric acid, etc.
4. Excellent resistance to corrosion of various inorganic acid mixed solutions
5. When the temperature reaches 40℃, it can show good corrosion resistance in various concentrations of hydrochloric acid solution
6. Good workability and weldability, no post-weld cracking sensitivity
7. Manufacture certification of pressure vessels with wall temperature of -196~450℃
8. Certified by the American Society of Corrosion Engineers NACE standard (MR-01-75) to meet the highest standard level VII for use in sour gas environments.
Inconel625 Application Areas
The softened and annealed low carbon alloy 625 is widely used in the chemical process industry, and its better corrosion resistance and high strength enable it to be used as a thinner structural component. Alloy 625 can be used in applications exposed to seawater and subject to high mechanical stress. Typical application areas:
1. Components of organic chemical processes containing chlorides, especially where acid chloride catalysts are used
2. Digesters and bleaching tanks for the pulp and paper industry
3. Absorption tower, reheater, flue gas inlet baffle, fan (humid), agitator, deflector and flue in flue gas desulfurization system
4. For the manufacture of equipment and components for use in sour gas environments
5. Acetic acid and acetic anhydride reaction generator
6. Sulfuric acid condenser
Product detail pictures:


Related Product Guide:
We not only will try our greatest to present fantastic expert services to each purchaser, but also are ready to receive any suggestion offered by our prospects for Discount Price Inconel 690 Tubes - Superalloy Inconel625/ UNS N06625/ Alloy625 Manufacturer – Guojin , The product will supply to all over the world, such as: Macedonia, Guatemala, Albania, Our factory is equipped with complete facility in 10000 square meters, which makes us be able to satisfy the producing and sales for most auto part products. Our advantage is full category, high quality and competitive price! Based on that, our products win a high admiration both at home and abroad.

In our cooperated wholesalers, this company has the best quality and reasonable price, they are our first choice.