Discount Price Nickel Superalloy Bar – Pure Nickel UNS N02200/ N6/ Ni200 Seamless Pipe, Sheet, Bar, Strip – Guojin
Discount Price Nickel Superalloy Bar – Pure Nickel UNS N02200/ N6/ Ni200 Seamless Pipe, Sheet, Bar, Strip – Guojin Detail:
Available Products
Seamless tube, Plate, Rod, Forgings, Fasteners, Pipe Fittings.
Production Standards
Product | ASTM |
Bar | B 160 |
Sheets, Sheets and Strips | B 162, B 906 |
Seamless Pipe and Fittings | B 161, B 829 |
welded pipe | B 725, B 775 |
Welded pipe fittings | B 730, B 751 |
Welded connectors | B 366 |
Forging | B 564 |
Chemical Composition
% |
Ni |
Fe |
C |
Mn |
Si |
S |
Cu |
Min |
99.5 |
|
|
|
|
|
|
Max |
|
0.40 |
0.15 |
0.35 |
0.35 |
0.010 |
0.25 |
Physical Properties
Density |
8.89 g/cm3 |
Melting |
1435-1446℃ |
Nickel 200 Material Properties
Nickel 200 (N6) has excellent corrosion resistance, high electrical vacuum performance and electromagnetic viewing performance, and is widely used in chemical, mechanical and electronic, food and other fields. Pure nickel has excellent welding performance and processing performance, and can be processed into pipe, rod, wire, strip, and foil products. It is one of the most widely used materials in industry. It has good mechanical properties and excellent corrosion resistance in many corrosion-resistant environments, especially caustic soda corrosion.
Nickel 200 (N6) is a commercially processed pure nickel that is effective against corrosion in a variety of chemical environments. It can also be used under oxidizing conditions to passively form an oxide film, making it extremely resistant to alkali metal corrosion. Nickel 200 (N6) is limited to use below 315°C, because the increase in temperature will cause graphitization, which will seriously damage its quality. In this case, Nickel 201 is required. It has a high Curie temperature and good magnetic properties. And its thermal conductivity and electrical conductivity are higher than nickel alloys.
Nickel 200 (N6) Material Application Areas
In food processing equipment, salt refining equipment. However, the equipment and the like required to manufacture industrial sodium hydroxide under high temperature conditions above 300°C. In the field of materials, it can be used to manufacture plates, strips, round bars, and welded pipes.
Food and synthetic fibers; electrical and electronic components; aerospace and missile components; chemical storage tanks.
Product detail pictures:



Related Product Guide:
Adhering to the principle of quality, service, efficiency and growth, we have gained trusts and praises from domestic and international client for Discount Price Nickel Superalloy Bar – Pure Nickel UNS N02200/ N6/ Ni200 Seamless Pipe, Sheet, Bar, Strip – Guojin , The product will supply to all over the world, such as: America, Denver, Austria, They are sturdy modeling and promoting effectively all over the world. Never ever disappearing major functions within a quick time, it's a have to for you of fantastic good quality. Guided by the principle of Prudence, Efficiency, Union and Innovation. the corporation. ake an excellent efforts to expand its international trade, raise its organization. rofit and raise its export scale. We are confident that we are going to have a bright prospect and to be distributed all over the world in the years to come.

High production efficiency and good product quality, fast delivery and completed after-sale protection, a right choice, a best choice.