Factory Price For Inconel 601 Bar - Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Seamless Pipe, Sheet, Wire – Guojin
Factory Price For Inconel 601 Bar - Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Seamless Pipe, Sheet, Wire – Guojin Detail:
Available Products
Seamless tube, Plate, Rod, Forgings, Fasteners, Pipe Fittings
Production Standards
Product |
ASTM |
Bars and Forgings |
B 637 |
Chemical Composition
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
S |
Ti |
Nb+Ta |
Al |
Co |
Cu |
Min |
70.0
|
14.0 |
5.0 |
|
|
|
|
2.25 |
0.70 |
0.40 |
|
|
Max |
17.0 |
9.0 |
0.08 |
1.00 |
0.50 |
0.010 |
2.75 |
1.20 |
1.00 |
1.00 |
0.50 |
Physical Properties
Density |
8.28 g/cm3 |
Melting |
1393-1427℃ |
Inconel X-750 Features
Inconel X-750 alloy is mainly a nickel-based superalloy which is age-strengthened with γ[Ni3(Al, Ti, Nb)] phase. It has good corrosion resistance and oxidation resistance below 980℃, and below 800℃ It has high corrosion resistance. It has good relaxation resistance below 540°C, as well as good formability and weldability. This alloy is mainly used for the manufacture of aircraft engines that work below 800°C and require high strength. . Springs can also be used to manufacture steam turbine turbine blades and other parts, such as plates, strips, bars, forgings, rings, wires, pipes, etc.
Inconel X-750 Heat Treatment Process
The solution heat treatment system for plates, strips and pipes in the supply state is 980℃±15℃, air cooling. For the intermediate heat treatment system of materials and parts, the following processes can be selected for heat treatment.
Annealing: 955~1010℃, water cooling.
Annealing of welded parts before welding: 980℃, 1h.
Stress relief annealing of welded parts: 900℃, moisturizing for 2h.
Stress relief annealing: 885℃±15℃, 24h, air cooling.
Inconel X-750 Available Varieties and Specifications
Bars, forgings, rings, hot-rolled sheets, cold-rolled sheets, strips, tubes and wires can be supplied in various sizes.
Plates and strips are generally supplied after hot or cold rolling, annealing or solution, pickling and polishing.
Bars, forgings and rings can be supplied in the forged or hot rolled state; they can also be supplied in solution treatment after forging; bars can be supplied after solution and polished or turned, and can be supplied in cold when the order requires Pull state into place.
The wire can be supplied in the solid solution state; for the wire with a nominal diameter or thickness below 6.35mm, it can be solid solution and supplied with a cold drawing deformation of 50% to 65%; the nominal diameter or side length is greater than 6.35mm. Wire, after solution treatment, is supplied with a cold-drawing deformation of not less than 30%. For wires with a nominal diameter or side length not greater than 0.65mm, they can be supplied with a cold-drawing deformation of not less than 15% after solution treatment as required.
Inconel X-750 Application Areas
The alloy is mainly used for the manufacture of leaf springs and coil springs with high strength requirements and relaxation resistance for aero-engines operating below 800°C. It can also be used to make parts such as turbine blades. Available varieties are sheet, strip, bar, forging, ring, wire and tube.
Product detail pictures:



Related Product Guide:
The organization upholds the philosophy of Be No.1 in good quality, be rooted on credit history and trustworthiness for growth, will keep on to provide previous and new customers from home and overseas whole-heatedly for Factory Price For Inconel 601 Bar - Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Seamless Pipe, Sheet, Wire – Guojin , The product will supply to all over the world, such as: Oslo, Ukraine, Vancouver, If you need to have any of our merchandise, or have other items to be produced, make sure you send us your inquiries, samples or in depth drawings. Meanwhile, aiming to develop into an international enterprise group, we look forward to receiving offers for joint ventures and other cooperative projects.

The company can keep up with the changes in this industry market, product updates fast and the price is cheap, this is our second cooperation, it's good.