Hot New Products Nickel Superalloy Tubes - Pure Nickel UNS N02200/ N6/ Ni200 Seamless Pipe, Sheet, Bar, Strip – Guojin
Hot New Products Nickel Superalloy Tubes - Pure Nickel UNS N02200/ N6/ Ni200 Seamless Pipe, Sheet, Bar, Strip – Guojin Detail:
Available Products
Seamless tube, Plate, Rod, Forgings, Fasteners, Pipe Fittings.
Production Standards
Product | ASTM |
Bar | B 160 |
Sheets, Sheets and Strips | B 162, B 906 |
Seamless Pipe and Fittings | B 161, B 829 |
welded pipe | B 725, B 775 |
Welded pipe fittings | B 730, B 751 |
Welded connectors | B 366 |
Forging | B 564 |
Chemical Composition
% |
Ni |
Fe |
C |
Mn |
Si |
S |
Cu |
Min |
99.5 |
|
|
|
|
|
|
Max |
|
0.40 |
0.15 |
0.35 |
0.35 |
0.010 |
0.25 |
Physical Properties
Density |
8.89 g/cm3 |
Melting |
1435-1446℃ |
Nickel 200 Material Properties
Nickel 200 (N6) has excellent corrosion resistance, high electrical vacuum performance and electromagnetic viewing performance, and is widely used in chemical, mechanical and electronic, food and other fields. Pure nickel has excellent welding performance and processing performance, and can be processed into pipe, rod, wire, strip, and foil products. It is one of the most widely used materials in industry. It has good mechanical properties and excellent corrosion resistance in many corrosion-resistant environments, especially caustic soda corrosion.
Nickel 200 (N6) is a commercially processed pure nickel that is effective against corrosion in a variety of chemical environments. It can also be used under oxidizing conditions to passively form an oxide film, making it extremely resistant to alkali metal corrosion. Nickel 200 (N6) is limited to use below 315°C, because the increase in temperature will cause graphitization, which will seriously damage its quality. In this case, Nickel 201 is required. It has a high Curie temperature and good magnetic properties. And its thermal conductivity and electrical conductivity are higher than nickel alloys.
Nickel 200 (N6) Material Application Areas
In food processing equipment, salt refining equipment. However, the equipment and the like required to manufacture industrial sodium hydroxide under high temperature conditions above 300°C. In the field of materials, it can be used to manufacture plates, strips, round bars, and welded pipes.
Food and synthetic fibers; electrical and electronic components; aerospace and missile components; chemical storage tanks.
Product detail pictures:



Related Product Guide:
abide by the contract, conforms on the market requirement, joins from the market competition by its good quality likewise as provides more comprehensive and superb support for customers to let them become large winner. The pursue of the company, is definitely the clients' pleasure for Hot New Products Nickel Superalloy Tubes - Pure Nickel UNS N02200/ N6/ Ni200 Seamless Pipe, Sheet, Bar, Strip – Guojin , The product will supply to all over the world, such as: Serbia, Victoria, Serbia, Our company offers the full range from pre-sales to after-sales service, from product development to audit the use of maintenance, based on strong technical strength, superior product performance, reasonable prices and perfect service, we will continue to develop, to provide the high-quality products and services, and promote lasting cooperation with our customers, common development and create a better future.

It is a very good, very rare business partners, looking forward to the next more perfect cooperation!